SPARK305LB
Master alloy for the production of yellow 375 – 417 – 585 ‰ gold jewellery obtained by investment casting. The elements contained in this product ensure a high deoxidation in casting and a high surface quality, making it suitable for castings with and without stones in place.
| 375 ‰ | 417 ‰ | 585 ‰ | ||
| Hardness as cast | 102 HV | 101 HV | 109 HV | |
| Density | 10.89 g/cm3 | 11.23 g/cm3 | 12.72 g/cm3 | |
| Melting Range | Solidus: 840 °C Liquidus: 910 °C |
Solidus: 824 °C Liquidus: 905 °C |
Solidus: 830 °C Liquidus: 880 °C |

375 ‰