PRIMA307NG

Master alloy for the production of yellow 875 – 917 ‰ gold jewellery obtained by investment casting. This product, thanks to its complex composition made of numerous different special elements, ensures an extreme level of deoxidation, an extreme surface quality, an enhanced fluidity and a long lasting of this features also after many reuses of casting scraps, making it the most advanced solution for castings with and without stones in place.

 

875 ‰ 917 ‰
Hardness as cast 129 HV 97 HV
Density 16.6 g/cm3 17.39 g/cm3
Melting Range Solidus: 787 °C
Liquidus: 893 °C
Solidus: 801 °C
Liquidus: 936 °C

 

Technical Data Sheet

875 ‰

917 ‰


Material Safety Data Sheet

MSDS

SKU: PRIMA307NG Category:

Description

PRIMA307NG

Master alloy for the production of yellow 875 – 917 ‰ gold jewellery obtained by investment casting. This product, thanks to its complex composition made of numerous different special elements, ensures an extreme level of deoxidation, an extreme surface quality, an enhanced fluidity and a long lasting of this features also after many reuses of casting scraps, making it the most advanced solution for castings with and without stones in place.

 

875 ‰ 917 ‰
Hardness as cast 129 HV 97 HV
Density 16.6 g/cm3 17.39 g/cm3
Melting Range Solidus: 787 °C
Liquidus: 893 °C
Solidus: 801 °C
Liquidus: 936 °C

 

Technical Data Sheet

875 ‰

917 ‰


Material Safety Data Sheet

MSDS

Additional information

Group

Color

Color gradient

Carat

,

Process

Family